(PDF) Highly efficient oxidation of Panzhihua titanium slag …
Since the contents of sulfur (S), phosphorus (P) and carbon (C) element were all below 0.030% in the prepared rutile TiO2 with the recommended roasting approach (roasted at 1100 °C for 120 min ...